Home > Steel News > Content
Properly Installed Carbon Steel Flanges
Sep 06, 2016

Excerpt: carbon steel flange after refining the molten steel is poured into ladles, turn through the turret to be pouring ladle to the tundish into the above, long nozzle injection of molten steel in tundish. Pei surface solidification of cast embryos after two cold forging training quickly cooled to a solid fixed length after cutting, thus completing the entire casting process. Depending on the steel grade can be done of mold oscillation processes and fluxes between the matches, thus achieving stainless steel fittings note Pei surface grinding rolling targets. Promoting small-scale water project management system reform in rural areas, enhance the vitality of grass-roots water conservancy development, guiding work around the small rural water project management system reform, actively guiding and promoting the development of farmer water users Association.

Carbon steel flange before installation, first check the pipes, pipe fittings and plastic quality is qualified, and wipe clean face and spigot. Sealing is completed, the fittings to dry for 20 minutes in order to achieve the best degree of sealing adhesive, to achieve the best sealing effect. Quality fittings and aprons failed: aprons, air holes, cracks, seams, apron because the curing time is too long or too short, resulting in elasticity of rubber ring is not ideal. Pipe system in place, the people fitting the user's experience, the establishment of a good pipe damage repair and maintenance system, guarantee the normal operation of civilian pipe. Carbon steel flanges and apron in the specified direction (in the upside, small end facing out) into the socket Groove shall not be distorted. After installation negligence no feeler Gage check, resulted in a rubber ring to launch expansion outside Groove.

Carbon steel flange after refining the molten steel is poured into ladles, turn through the turret to be pouring ladle to the tundish into the above, long nozzle injection of molten steel in tundish. Pei surface solidification of cast embryos after two cold forging training quickly cooled to a solid fixed length after cutting, thus completing the entire casting process. Depending on the steel grade can be done of mold oscillation processes and fluxes between the matches, thus achieving stainless steel fittings note Pei surface grinding rolling targets. Promoting small-scale water project management system reform in rural areas, enhance the vitality of grass-roots water conservancy development, guiding work around the small rural water project management system reform, actively guiding and promoting the development of farmer water users Association.

Previous: Flange Jar Link Properties

Next: No Information